> Dear friends
> Pls confirm with reference to ASME Sec VIII-1
>
> Up to -29°C MDMT, if impact test is exempted as per ASME code then we need not to see whether weld consumables are impact tested to that MDMT.
>
> Same is applicable to raw materials viz plate, pipe, flanges, if at -29°C, impact test is exempted, then MTC need not to show impact test results at that MDMT -29°C.
>
> Aly
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments