Thursday, February 6, 2014

Re: [MW:20030] Re hydrotest for surface packages

Dear Sridahr

Hydro test purpose  is to check Strength and Leakage on Assembly. if you do hydro test without assembly , it will very difficult to judge abt assembly stiffness / strength  against standard  pressure as per applicable code .

If i will be your client , i will not waiver hydro test .

Thank you very much 
\
Best of regards

Ritesh Rajput 


On Thu, Feb 6, 2014 at 11:05 AM, Kumar <sk7920541@gmail.com> wrote:
Dear Sridhar,

The hydrostatic pressure testing is mainly to check the mechanical
integrity of weld joints & to asses the same for the base metal as
well. So, in your case if there are no new weld joints, hydrotest
could be waived. but you may have to do leak test (at operational
pressure) for the new flanged (with gaskets) in order to check the
leak proofing.this is just for info.
Regards,
Kumar
On 2/5/14, Sridhar Doddapaneni <sridhar.doddapaneni@gmail.com> wrote:
> Refer B 31.3, it allows ndt for that weld joint lieu of hydro test.
> Normally that type of joints called as golden joints.
>
> Sridhar
> On Feb 5, 2014 12:00 PM, "antony jenis" <antonyjenis@gmail.com> wrote:
>
>> Gent's
>>
>> We have the 3 different skids fabricated and hydrotested at 3 different
>> locations but assembly will be at 1 location .For this the loose shipping
>> spools will be hook up at the assembly location . Is there any
>> requirement
>> for re hydrotest for the assembled full package.
>>
>> Thanks and regards
>> Antonyjenis
>> Abudhabi
>> 00971505624002
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>>
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>
>> The views expressed/exchnaged in this group are members personel views
>> and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>> ---
>> You received this message because you are subscribed to the Google Groups
>> "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an
>> email to materials-welding+unsubscribe@googlegroups.com.
>> For more options, visit https://groups.google.com/groups/opt_out.
>>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...