Re: [MW:20011] Side wall lack of fusion

Dear,
Lack of fusion with side wall in butt joint you can go through by following methods...
Method-1- Take section form test piece, grind smooth finish and perform Macro-eatch test.
Method -2-  Take section form test piece, take test for 90 deg bending test at each side wall.

Thanks and regards,
Bhagwat Ambule.


On Friday, 10 January 2014 8:32 AM, Sara Vana <krmech2000@gmail.com> wrote:
Dear experts,
How to measure side wall lack of fusion by destructive testing.
Component : butt welding of plates
Joint configuration : groove weld with included angle sixty degree
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...