Re: [MW:19999] RE: 19992] PWHT AND TEMPERING OF LAS GR 11

Yes, Material is SA 182 F11 CL2

Prasad

On Feb 4, 2014 9:08 AM, "Shashank Vagal" <nach_sam@yahoo.com> wrote:
Hi Prasad,
Please give UNS No. for this material, is it by any chance SA-182 F11 Cl2, UNS K11572, 1-1/4 Cr 1/2 Mo?
 
With Best Regards,
Shashank C Vagal 


On Tuesday, 4 February 2014 8:32 AM, Antonio Diaz <aada@unam.mx> wrote:
Your client requires to get a hardness a little lower than hardness tempering. You should verify both hardnes material for tempering and pwht.

De: Prasad
Enviado: 03/02/2014 16:26
Para: materials-welding@googlegroups.com
Asunto: [MW:19992] PWHT AND TEMPERING OF LAS GR 11

WE HAVE FORGING FLANGES TO SA 182 GR11 Cl2 MATERIAL RECEIVED IN NORMALIZED AND TEMPERED CONDITION.
TEMPERING IS DONE AT 660 deg. C BY FORGING MANUFACTURER.
AFTER WELDING FLANGES COMPLETE EQUIPMENT POST WELD HEAT TRETEAD AT 660deg. C. AS PER ASME Sec VIII DIV. 1.
AS PER CLIENT SPEC. THERE SHOULD BE MINIMUM DIFFERENCE OF 20 deg. C IN TEMPERING & PWHT TEMPERATURE

WILL THIS PWHT TEMPERATURE WILL HAVE ANY ADVERSE EFFECT ON FORGINGS.

EXPERTS VIEWS ARE REQUESTED TO RESOLVE THIS ISSUE AND SOLUTION FOR ACCEPTANCE OF COMPLETED EQUIPMENT.

THANKS,

P.GHANEKAR
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...