Sunday, June 30, 2013

Re: [MW:18047] External reinforcement for pipeline

It means the reinforcement must be greater than the pipe surface n less than 1.6 mm. If it is greater than 1.6mm u can grind it for a little circumferential length, but normally the client will not allow..n itz not a good practice too..so insist the welders to weld with a reinforcement below the specified.

Binu valiyaveedu

On 29 Jun 2013 13:01, "anhtrangnghieng" <anhtrangnghieng@gmail.com> wrote:

Dear Experts,

 

I am working to fabricate tie-in spools for pipeline and applicable standard is API 1104

As per API 1104:  7.8.2 Filler and Finish Beads : At nopoint shall the crown surface fall below the outside surface ofthe pipe, nor should it be raised above the parent metal bymore than 1/16in. (1.6 mm).

 

This means : Weld metal: the external reinforcements must not exceed the indicated dimensions ( 1.6 mm) /therefore,  if external reinforcement exceed 1.6 mm, The external reinforcement must be removed to below 1.6 mm as API 1104 required.

 

Please help me to clarify this doubt/

 

Thanks/


--




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...