It certainly is permissible to write a properly supported WPS with multiple conditions.  However, one starts to get into a booking keeping nightmare if one is not very, very careful.  You must provide clear instructions on the applicability so you don’t get into deep trouble due to misapplication.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ahmed Husain
Sent: Tuesday, June 25, 2013 11:18 AM
To: materials-welding@googlegroups.com
Subject: Fw: [MW:18038] WPS with multiple PQR

 

It means, It is not correct to prepare a WPS supported my multiple PQR, with two condition, i.e. with PWHT and without PWHT. Also, instead of using two WPS on one joint, a new WPS is required to be prepared combining both WPS.

 

Please correct me if I am wrong.

 

Regards,

A, Husain

 

----- Forwarded Message -----
From: joseph mbé <mbejoseph@yahoo.fr>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Monday, June 24, 2013 11:06 AM
Subject: Re: [MW:18018] WPS with multiple PQR

 

see my answer here below in red

 

Joseph Faustin Mbe

QA/QC Engineer

TEL CMR (00237) 33129846

TEL CG (00242) 057388009

BP 1155 Pointe Noire

Yesterday is the pass, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

 

 

De : Ahmed Husain <ahmraha@yahoo.com>
À : "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Envoyé le : Dimanche 23 juin 2013 17h00
Objet : [MW:18005] WPS with multiple PQR

 

Dear All, 

 

Followings are brief details of five PQRs.

PQR No.                 Process                       Base metal                             B.M. Thick      B.M. RANGE              PWHT                         Impact

 

#1                     SMAW                        P1Gr3 to P1Gr3                      0.24 Thk         1.6 -12                        N/A

#2                    SMAW                        P1GR3-P1GR2                        0.24 Thk          1.6 -12                         N/A                              YES (-51 F)

#3                    SMAW                        P1Gr3 to P1Gr3                      1.5 THK           16 - 200                       1150/10 HRS              YES (-51 F)

#4                    SMAW                        P1GR3-P1GR2                        1.5 THK           16 - 200                       1150/08 HRS               ES (-60 F)

#5                    SMAW                        P1Gr3 to P1Gr3                      1.75 THK         16 - 200                       N/A                              YES (-51 F)

 

 

Based on above PQRs,

 

1.    Is it acceptable to prepare  a single  WPS with two welding condition ( with and without PWHT), with notes stating thickness limits for both conditions. (why not 2 different wps )

2.    If yes, what would be thickness range for welding with & without PWHT. (PWHT is an EV so, not possible for my knowledge)

3.    With reference to ASME IX- QW-200.4 Combination of Welding Procedures,: If a company has two WPS, one in GTAW process and second in SMAW process, is it acceptable to apply individually both WPS on single joint? Or new WPS will be required combing both WPS? (Are you talking about 02 PQR or 2 WPS? if 02 PQR, Yes it's possible to use the combination of 02 PQR qualified separately but, in the limite of tickness range for each process). 

 

 

 Your valuable feedback will be highly appreciated.

 

Regards,

A.Husain

 

 


The contents of this email, including all related responses, files and attachments transmitted with it (collectively referred to as “this Email”), are intended solely for the use of the individual/entity to whom/which they are addressed, and may contain confidential and/or legally privileged information. This Email may not be disclosed or forwarded to anyone else without authorization from the originator of this Email. If you have received this Email in error, please notify the sender immediately and delete all copies from your system. Please note that the views or opinions presented in this Email are those of the author and may not necessarily represent those of Saudi Aramco. The recipient should check this Email and any attachments for the presence of any viruses. Saudi Aramco accepts no liability for any damage caused by any virus/error transmitted by this Email.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...