Tuesday, June 25, 2013

Re: [MW:18034] Re: phased array vs. RT

NDE / NDT Methods are generally classified as surface methods (PT, VT) surface and subsurface methods (MT, ET) and Volumetric Methods (RT, UT) depending on their ability to detect discontinuities located at different depths below the surface of the test material. Volumetric methods are able to detect the presence of discontinuities if any throughout the volume of the given test material. 

If you need any more information, feel free to contact me.

Regards

Swamy

On Tuesday, June 25, 2013 9:54:13 AM UTC+5:30, kaku wrote:
Dear Sir,
 
What is the meaning of Volumetric NDE?
 
Thanks,
 


 
On Tue, Jun 25, 2013 at 9:42 AM, veera raghava kommisetti <kommi...@gmail.com> wrote:
Volumetric exmaination in-lieu of RT is allowed by code.
PA falls under Volumetric examiantion.
Best option would be PA+ToFD


On Tue, Jun 25, 2013 at 7:31 AM, Raghuram Bathula <raghura...@gmail.com> wrote:
http://www.linkedin.com/groupAnswers?viewQuestionAndAnswers=&discussionID=144891298&gid=122787&commentID=146402448&trk=view_disc&ut=1PWB0HnGhwYRM1

Interesting discussion on the above topic

On Tuesday, December 7, 2010 1:30:16 PM UTC+5:30, Navid Navidi wrote:
Hi all,

is it possible to use phased array technique instead of RT for NDT teast of a pressure vessels.
Does standard allow us to do so?
what is its advantages?

thank you in advance
Saeed

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...