Re: [MW:18010] FCAW Weaving Width

When your client says 20 mm  is not acceptable, then pl. find out what is their acceptable norms.

Calculate the total width of cap run and use 3 layers in place of  2 layer deposit.

This will help to increase the travel speed (due to reduced width of each layer) and also avoid NCRs.

Sridhar.



From: Ram Chatt <chattru@gmail.com>
To: materials-welding@googlegroups.com
Cc: c sridhar <sridhar305@yahoo.com>
Sent: Monday, 24 June 2013 8:34 AM
Subject: Re: [MW:18007] FCAW Weaving Width

Thank you Friend,
 
 
in my problem we are welded so many joints for FCAW welding weaving width for single layer 20-25 mm (using multi 2 layer welding totaly caping width 45-48 mm ).But our client said this is not allowable .they make NCR.

 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...