Sunday, June 23, 2013

Re: [MW:18009] WPS with multiple PQR

Q1 - No
Q2- N/a
Q3- You need write new WPS by combining existing WPS (No new PQR required)


On Sun, Jun 23, 2013 at 8:00 PM, Ahmed Husain <ahmraha@yahoo.com> wrote:
Dear All, 
 
Followings are brief details of five PQRs.
PQR No.                 Process                       Base metal                             B.M. Thick      B.M. RANGE              PWHT                         Impact
 
#1                     SMAW                        P1Gr3 to P1Gr3                      0.24 Thk         1.6 -12                        N/A
#2                    SMAW                        P1GR3-P1GR2                        0.24 Thk          1.6 -12                         N/A                              YES (-51 F)
#3                    SMAW                        P1Gr3 to P1Gr3                      1.5 THK           16 - 200                       1150/10 HRS              YES (-51 F)
#4                    SMAW                        P1GR3-P1GR2                        1.5 THK           16 - 200                       1150/08 HRS               ES (-60 F)
#5                    SMAW                        P1Gr3 to P1Gr3                      1.75 THK         16 - 200                       N/A                              YES (-51 F)
 
 
Based on above PQRs,
 
1.    Is it acceptable to prepare  a single  WPS with two welding condition ( with and without PWHT), with notes stating thickness limits for both conditions.
2.    If yes, what would be thickness range for welding with & without PWHT.
3.    With reference to ASME IX- QW-200.4 Combination of Welding Procedures,: If a company has two WPS, one in GTAW process and second in SMAW process, is it acceptable to apply individually both WPS on single joint? Or new WPS will be required combing both WPS?
 
 
 Your valuable feedback will be highly appreciated.
 
Regards,
A.Husain
 


The contents of this email, including all related responses, files and attachments transmitted with it (collectively referred to as "this Email"), are intended solely for the use of the individual/entity to whom/which they are addressed, and may contain confidential and/or legally privileged information. This Email may not be disclosed or forwarded to anyone else without authorization from the originator of this Email. If you have received this Email in error, please notify the sender immediately and delete all copies from your system. Please note that the views or opinions presented in this Email are those of the author and may not necessarily represent those of Saudi Aramco. The recipient should check this Email and any attachments for the presence of any viruses. Saudi Aramco accepts no liability for any damage caused by any virus/error transmitted by this Email.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...