Friday, June 21, 2013

Re: [MW:17996] Clarification on Current and Polarity Abbreviations

Current ( electron) flows from Negative to Positive . When Electron hits the +ve, more heat (2/3) is generated in +ve terminal( say holder)


On Thu, Jun 20, 2013 at 6:02 PM, jiji lal <jijilalkm@gmail.com> wrote:
Dear Anban,
 polarity related to the flow direction of current in a welding circuit.
Technically , we assume the current starts flowing from +ve terminal of the power source then  returns through -ve terminal and hence the item(electrode/parent metal) wchich connects in +e terminal can produce more heat(66%) than -ve(33%).

In DCSP Electrode will connect to -ve terminal only ,so in other means we can say  DCSP= DC-VE= .DCEN
In DCRP Electrode will connect to +ve terminal only ,so in other means we can say DCRP= DC+VE= DCEP
Regards
Jijilal K M,
Tecpro Infra projects Ltd.
Kochi. S.India


On Tue, Jun 18, 2013 at 3:16 PM, Anban <gane2478@hotmail.sg> wrote:

Dear Experts
Pls enlighten me if thse abbr. are same and explain the correlation and difference


1 -  DCEP x DC+VE  x DCSP
2 -  DCEN x DC-VE x DCRP

DCEP - Direct Curent Electrode Positive
DCSP - Direct Current Straight Polarity
DCRP - Direct Current Reverse Polarity

Appreciation in advance

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...