Wednesday, June 19, 2013

Re: [MW:17979] Problem in welding of IS2062 with IS276 GR1(Austenitic Mangnese steel).



Please send the mechanical properties of IS 2062 and IS 276 which materials you have used then
which filler materials you used what was the thickness have you tested PQR/

On Wed, 19 Jun 2013 09:41:17 +0530 wrote
>We are doing welding of IS2062 with IS276 GR1(Austenitic Mangnese steel)..During Transverse
tensile material failed in HAZ area and we are getting 319 MPa UTS but we need about 500
MPa.Plz suggest...


Abhishek Singh



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>

>
The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
>
---
>
You received this message because you are subscribed to the Google Groups "Materials &
Welding" group.
>
To unsubscribe from this group and stop receiving emails from it, send an email to materials-
welding+unsubscribe@googlegroups.com.
>
For more options, visit https://groups.google.com/groups/opt_out.
>

>

>


Dear Sir,





Thanking You.

With Warm Regards,

Muthu barathi P,
Mobile No. +918511180665

Get your own FREE website and domain with business email solutions, click here

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...