RE: [MW:17964] BASEMATERIALIMPACTTESTINGREQUIREMENT

Dear Saravanan,

Pls. refer UG 84 ( c) (5)

 

UG-84(c)(5) For all Charpy impact tests the following

test temperature criteria shall be observed:

(a) For Materials of Nominal Thickness Equal to

or Greater Than 0.394 in. (10 mm). Where the largest

obtainable Charpy V-notch specimen has a width along

the notch of at least 0.315 in. (8 mm), the Charpy test

using such a specimen shall be conducted at a temperature

not warmer than the minimum design metal temperature.31

Where the largest possible test specimen has a width along

the notch less than 0.315 in. (8 mm), the test shall be

conducted at a temperature lower than the minimum design

metal temperature31 by the amount shown in Table

UG-84.2 for that specimen width. [This latter requirement

does not apply when the option of (c)(2)(a) above is used.]

 

Hope this will be helpful

 

Cheers

MM

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Saravanan Sornam
Sent: Tuesday, June 18, 2013 9:20 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:17957] BASEMATERIALIMPACTTESTINGREQUIREMENT

 

Hi Mr.Veera ,

 

Could U pls tell me the clause no. in ASME VIII Div I , as per your statement, i wanted to confirm this.

 

Regards,

Saravanan

 

On Tue, Jun 18, 2013 at 1:40 PM, veera raghava kommisetti <kommisetti@gmail.com> wrote:

Since 7.5 is less than 80% of base metal thickness (8mm), you need to do impact test at -45 + (-3) = -48 Deg

 

On Mon, Jun 17, 2013 at 7:55 PM, Ankit Gandhi <asgandhi.90@gmail.com> wrote:

Dear Expert,

We are making a vessel according to ASME Sec. VIII Div. 1
MDMT is -45 Degree .C
Thickness 10 mm
Now, If i am using Impact specimen size 7.5 than I have to reduce the Impact Temperature? & yes then How much?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...