Step 1) See ASTM B466 have 3 no. of Grades - C70600, C71000, C71500, hence P No. is 34 for these . Refer ASME -IX, QW-422 .

Step 2 ) Refer ASME II C, SFA 5.7 , AWS Class ERCuNi , to weld the above B466 all Grades. Also attached sample Filler Data for your reference.

Step 3)  Then, go back to ASME -IX, Refer QW-432 for Cu & its Alloys, ERCuNi , SFA 5.7 shows F No. 34.



Hope it helps and Sorry if I did any mistake..

Regards,
Saravanan


On Tue, Jun 18, 2013 at 12:45 AM, suthan mr <suthan.mr@gmail.com> wrote:
Hi friends,

For example, ASTM B466 it's the cu-Ni alloy material.How to find the F-number, what are the section to be referred?


Kindly send the brief explanation...

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...