Wednesday, April 17, 2013

Re: [MW:17450] Weld Seam & drain point overlapping...

This is quite common specially with equipment
After welding as per ASME xiii RT shall be carried out on the weldolet welding as well as two additional shots 3 inches either side of the weldolet welded
I hope this helps

Sent from my iPhone 
Regards B. Alavi

On 16 Apr 2013, at 18:19, ABHISHEK GHOSH <ghoshabhishekmech@gmail.com> wrote:


Dear Experts , 

Weldolet ( Drain point ) is overlapping Long  seam of 48 inch  90 deg LR Elbow .. 
Design pressure : 96  Bar
Design temp ( Max/Min) : 80/5 deg C
Hydrotest Pressure : 120 Bar 
NDT : 100 % RT , MPI 
Application : Subsea 
Service: Offshore Non Sour, Non Corrosive , HC Crude Blended Oil 
Spec : ASME B 31.4 

Elbow Spec: ASTM A 860 WPHY 65 WLDD 

Kindly refer attached snap .. 

My Question is what should be the NDT to be performed before & after welding of weldolet ? please put code/client  reference .. ( Any ) 

( Kindly let me know if more information is required) 

Thanks & regards.  

ABHISHEK GHOSH 


 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 
<IMG_0879.JPG>

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...