Re: [MW:17427] QUALIFYING ALLOY WELDERS ON CS PIPE

If the welder is used for Welder Qualification of Base metals from P.No. 1 to 15F, then the Welder is Qualified to weld the Base metals of P.No 1 through 15F as per ASME Sec IX QW-423.1.

Regards,

Karthikeyan


On Mon, Apr 15, 2013 at 4:29 PM, Zakaria ghrab <zakaria.ghrab@gmail.com> wrote:
Concerning Base material, you can,  Check just Filler metal F number according ASME sect IX.

Regards.


2013/4/14 Binoy Soman <binoy.spp@daelim.co.kr>

Dear Experts,

I want to qualify some welders for alloy welding (P3,P4,P5A,P15E). But we don't have alloy pipes. Can I do welder qualification test on CS Pipes.

 

S.Binoy

 

 

Thanks & Regards,

 

S.Binoy

Welding Engineer

Tel # (+966)-592633853

Shoaiba II CCPP Project

Saudi Arabia Co. Ltd.

                   

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
زكرياء غراب
GHRAB Zakaria
Jorf Lasfar Units 5&6 Power Plant construction Project
EA2C/ SDEM Entreprises
Site QA/QC Manager
Mobile : Morocco (+212) 6 61 07 00 11
             Tunisia (+216) 96 635 805



Yesterday is the pass, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
Thanks & Regards,
 
Karthikeyan. P,
Surveyor.
 
BUREAU VERITAS (INDIA) PRIVATE LIMITED,
30/6, 3rd Floor, Aparna Tower, New Dhamu Nagar,
Puliakulam Road, Pappanaiken Palayam,
Coimbatore - 641 037, India.
 
Mobile No.: 9994999503

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...