Monday, April 15, 2013

Re: [MW:17391] Request to provide filler metal & Flux combination for SAW process for low temperature service with Heat treatment

I suggest to go with F7P8 because he is asking for pwht also further filler shall be EH 14 because it contains higher Mn  to provide good impact properties

On Apr 11, 2013 10:22 AM, "Aly" <mhaskar.aly@gmail.com> wrote:

Dear Experts,

We are going to qualify welding procedure of following details

 

1.       Welding with

·         GTAW with ER70S2

·         SMAW with E7018-1 &

·         SAW

 

2.    Heat treatment after welding at 620°C @ 200min

3.    Impact testing after heat treatment at -46°C

 

Kindly  advise on  filler metal & Flux combination for SAW process to achieve impact properties after heat treatment.

 

Can F7A8 EM12K  will this serve the purpose…!!

 

 

Thanks & regards

 

Ali Mhaskar,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...