Hi, from my understanding, peaking and banding will be either negative or positive and depends where you hold he template, whether it is inside the tank or outside as it is not stated, if this has to be measured from a particular side of the tank.
It reckon it is surely + or -.
Am sure someone more experienced will throw some more light.


From: BINOY <binoyvtc@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Saturday, 13 April 2013, 20:42
Subject: [MW:17367] Peaking of tanks

Gents,

In API 650 it states that the value shall not exceed 13mm. my doubt is
if we get a value in negative it is acceptable.It is not clearly
stated that the value is + or -13mm.

please advise.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.




No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...