RE: [MW:17340] Pipe joint resting on the beam

My opinion is it is unsafe and because rain/moisture can accumulate on the beam it will lead to corrosion on the pipe.  Also, visual inspection cannot be perform 100% when doing routine inspection.



Jean Staton

Corporate RSO

Quality, Safety, Environmental Manager

 

METCO - Materials Evaluation & Technology Corporation

27 Sawyer St, Beaumont, TX 77702

Phone: (409) 835-2600

Fax:  (409) 835-1199

Cell:  (409) 553-9460

Email: jean.staton@metco-ndt.com

Website:  www.metco-ndt.com

 

 

 

 

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sumod s
Sent: Wednesday, April 10, 2013 4:55 AM
To: materials-welding@googlegroups.com
Subject: [MW:17330] Pipe joint resting on the beam

 

sir,

 

Please explain the basic reason for not permitting the practice as seen in attached photo.

 

sumod

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



DISCLAIMER: The information contained in this e-mail may be confidential and is intended solely for the use of the named addressee. Access, copying or re-use of the e-mail or any information contained therein by any other person is not authorized. If you are not the intended recipient please notify us immediately by returning the e-mail to the originator.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...