Dear Mr.Hemat
Use ER 309LMo with 99.99% argon for purging or ER 320LR
Regards
Sarfaraz
QAQC Engineer
On 4/6/13, hemant <hsuthar@chemithon.co.in> wrote:
> Dear All,
>
> We r going to weld SB -729 Pipe to SA312 TP 316L Pipe.
>
> We have to prepare new WPS . anybody can suggest me which filler wire we
> have to use for GTAW.
>
>
>
> Pls reply ASAP.
>
>
>
>
>
> Regards
>
> Hemant H suthar
>
> Asst. Manager QA/QC
>
> Chemithon Engineers Pvt Ltd.
>
> Khanvel-Kheradi Road. Silvassa, UT of DNH
>
> Website: <http://www.chemithon.co.in/> www.chemithon.co.in
>
> Office Contact: 0260 2677889 / 2677036 , 37 Cell : 9712973092
>
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>
--
Regards
TAMBE Sarfaraz.
mob. 9960860167
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Subscribe to:
Post Comments (Atom)
[MW:34919] Welder qualification certificate
Dear All anyone can share a format for welder certificate and card format Thanks & Best Regards Saleem manhappulath Mob:+9665...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment