Dear,

 

ER NiCr-3 can be used

 

S.Binoy

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of hemant
Sent: Saturday, April 06, 2013 11:11 AM
To: materials-welding@googlegroups.com
Subject: [MW:17297] SB-729 ALLOY-20 MATERIAL WELDING CONSUMABLE.

 

Dear All,

We r going to weld SB -729 Pipe to SA312 TP 316L Pipe.

We have to prepare new WPS . anybody can suggest me which  filler wire we have to use  for GTAW.

 

Pls reply ASAP.

 

 

Regards

Hemant H suthar

Asst. Manager QA/QC

Chemithon Engineers Pvt Ltd.

Khanvel-Kheradi Road. Silvassa, UT of DNH

Website: www.chemithon.co.in

Office Contact: 0260 2677889 / 2677036 , 37 Cell : 9712973092

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...