Dear Mr.Son,
Yes, I'm Vietnamese and nice to see you :).
Thanks for your advice but what I need 's spec to refer and how to
check the valve seal leaking because the valve is installed in series.
On 4/2/13, truong son bui <truongbs70@gmail.com> wrote:
> Dear Toan,
> Are you Vietnamese ? This is first time I see Vietnamese in this forum and
> is great.
> Your problem is simple: after welding, the welded valve may be inefficient
> by heating (shrink, crack ...) by slag. Those cause should make the valve
> be impaired.
> Inorder to sure it's functionality has been perfect, you should prepaire a
> temporary spool or hose and hydrolic pump ... for testing according by it's
> functionality. The testing proceduce should be approval by QA authorised.
> Wish success to you.
>
> On Mon, Apr 1, 2013 at 8:55 AM, toanvnguyen
> <nguyenvantoan221@gmail.com>wrote:
>
>> Dear Experts,
>>
>> We're doing a PLEM and TPAM project. The type of valves's welded-in
>> valve.
>> In spec. require as follow: "After fabrication's complete, welded-in
>> valves
>> shall be subject to seal tests in accordance with the relevant project
>> valve specification to demonstrate the valve functionality has not been
>> impaired during fabrication".
>> Could you pls give me some advice about this kind of tests. Many thanks.
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>>
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>
>> The views expressed/exchnaged in this group are members personel views
>> and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>> ---
>> You received this message because you are subscribed to the Google Groups
>> "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an
>> email to materials-welding+unsubscribe@googlegroups.com.
>> For more options, visit https://groups.google.com/groups/opt_out.
>>
>>
>>
>
>
>
> --
> Bui Son Truong - Director
> LILAMA Consultant Co.
> Address: 124 Minh Khai street, Hai Ba Trung Dist., Ha noi, Viet Nam.
> Fax: +84 3624 9416
> Tell: +84 3624 94 15
> Mobi:+84 9034 888 39
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>
--
Best Regards,
--------------------------------------------
Nguyen Van Toan
Piping & Machine Supervisor
Structure WS 2
- PTSC M&C
HP: 0907496198
email: toanvnguyen@ptsc.com.vn
Skype: toan_ptsc_mc
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Subscribe to:
Post Comments (Atom)
[MW:34920] Tubesheet Hole step
Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP -- https://materials-...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
1 comment:
Dear Toan,
You may find spec according to B16.34 or API 598
Those include test classes for seal and seat valve testing
------------------------
Nguyen Si Thang
QA
Member of Indutrade AB Key Valve Technologies Ltd.
2169-8, Jungwang-Dong, Shiheung-City
Gyeonggi-Do,
429-450 Korea
Tel. +82-31-363-0700
Direct tel. +82-31-363-0733
Mobile +82-10-2713-2332
Fax +82-31-496-0752
E-mail thang@keyvalve.com
Post a Comment