Yes to both.  An impact qualified procedure is essentially a subset of qualified procedures for the material/process/filler metal etc.;  i.e. a procedure with restrictions over and above those required for the more general condition. 

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ahmed Husain
Sent: Sunday, April 14, 2013 12:44 PM
To: materials-welding@googlegroups.com
Subject: [MW:17393] WPS

 

Dear All,

 

Your valuable comment is required on following cases.

 

1. Suppose, if i have a certified PQR for P1 Gr1 to P1Gr1 material with PWHT and impact testing. Process is GTAW and SMAW. Based on this PQR, can I prepare a WPS without impact testing, i.e for materials and design condition doesn't require impact testing. There is no issue in other variables.

2. Is it acceptable to apply a 'WPS prepared and approved for low temperature service with impact testing ' to a job, for which there is no requirement for impact testing.

 

A. Husain
ABS Consulting Inc.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...