[MW:17332] RE: 17328] PWHT for Gr. P91/P22/P11 during welder qualification

Assuming you are qualifying to ASME Section IX, you may qualify weldors using QW-423 for alternate base metals and of course using the correct F-number filler metal/electrode.  For example,  you would not be required to use Alloy 91 base metals and –B9 filler metals to qualify a weldor for welding Alloy 91.  (Same for other Cr-Mo materials).  QW-423 would allow qualification for welding Alloy 91 by performance testing with carbon steel (most common choice) base metals and with E7018 (17, 16) for SMAW, ER70-S X for GTAW, PAW, or GMAW.  Note that SAW, machine/automatic are not dependent on filler metal or base metal, i.e. are not essential variables for this process type.

 

If you chose to qualify weldors on the specific materials and with filler metals to be use in fabrication, then I would recommend that test coupon(s) be examined by volumetric examination per the requirements of QW-302.2 and QW-304(when permitted).

 

Let me know if you have further questions.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Binoy Soman
Sent: Wednesday, April 10, 2013 3:48 AM
To: materials-welding@googlegroups.com
Subject: [MW:17328] PWHT for Gr. P91/P22/P11 during welder qualification

 

Dear experts,

 

We know that PWHT can be avoided for  welder qualification (Ref:QW-301.2) even if WPS has PWHT. My doubt is whether it is required to do PWHT while performing welder qualification for Gr. P91/P 22/ P11. Kindly clarify.

 

S.Binoy

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...