Thanks for reply.

As My client suggested to do in Auto TIG , But my doubt is whether Manual TIG will give the Required property as that AUTO TIG for MARAGING STEEL 250?

plz suggest the difference and problems encounter.

On Fri, Feb 15, 2013 at 12:23 PM, vineet kumar <vineet.rdb@gmail.com> wrote:
DEAR,

REPLY IN RED  TO YOUR QUERIES.

1) What type of Process can be used ? TIG or MIG - TIG MORE PREFERABLE
2) What type of Consumables can be used? CONSUMABLE SHALL BE SAME AS BASE METAL COMPOSITION
3) What type of gases to be used and their Purity Level? - ARGON HIGH PURITY LEVEL
4) Heat Treatement ? - NO PREHEATING &  PWHT IN TWO STEP A) SOLUTION TREATMENT AT 820 C FOR 1 hr B) FULL AGEING TREATMENT AT 480 C FOR 3 hr.
5) what are the welding conditions to be followed when welding this steel?-  A) HIGH HEAT INPUT ARE AVOIDED  B) ELEVATED TEMP. FOR LONG PERIOD IS AVOIDED C) DONOT PREHEAT & KEEP INTERPASS BELOW 250 F.

REDARDS,
VINEET  KUMAR


On Thursday, February 14, 2013 6:09:30 PM UTC+5:30, Gopalakrishnan G wrote:
Can Any one Suggest me the weldability of Maraging Steel 250 ( ASTM A 579 Grade 72).Thaickness - 8 mm ( Full Penetration)

1) What type of Process can be used ? TIG or MIG
2) What type of Consumables can be used?
3) What type of gases to be used and their Purity Level?
4) Heat Treatement ?
5) what are the welding conditions to be followed when welding this steel?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
G.Gopalakrishnan
Welding Engineer
Mukand Ltd
Mumbai
Moble :+91-9833397917

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...