Pls. see link to NORSOK:

http://www.standard.no/en/Sectors/Petroleum/NORSOK-Standard-Categories/M-Material/M-6503/

 

1.Here you will see that rev. 4, 2011 is latest one, and you can just open/download it from the site (ref. the link).

2. On same site you will see a “frequently asked questions”, that answers it regarding the qualification process and who accepts the QTR.

3. See the scope in M-650. It may apply for A105, if A105 is in critical service. But otherwise there are no NORSOK std. for qualification of “usual products” including A105, A350 LF2, etc.

 

regards

Kristian

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kaz Williams
Sent: 9. februar 2013 20:26
To: materials-welding@googlegroups.com
Subject: [MW:16732] NORSOK

 

Dear My Friends:

1.What is the last revision of NORSOK M-650,? actually I have Rev.3 2004. Is this the last rev?

2.is it correct to ask an international Inspection  company to evaluate  products of a producer to issue  NORSOK approval?  Can Inspection company issue NORSOK approval based on M-650?

3.what is the NORSOK std for approval  a  producer for A105 , A350LF2 , A182 F11,22 material?

 

Regards

KWS

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...