Hi

refer to API RP 582. It has a table of selecting filler metal according to type of material to be welded.

Regards
Purav Desai

On Feb 8, 2013 8:34 PM, "Prakash Hegde" <pb.hegde@yahoo.com> wrote:
Hi!
For 13% Cr material i) If design temp is below 350C it is better to use 309MoL  ii) If design temp is higher It is better to use Inconel filloer i.e NCrFe2 or NiCrFe3 , or NiCrMo3
Regards
 
Hegde Prakash
Pune


--- On Fri, 8/2/13, kannayeram gnanapandithan <kgpandithan@gmail.com> wrote:

From: kannayeram gnanapandithan <kgpandithan@gmail.com>
Subject: Re: [MW:16722] welding of 13% cr steel
To: materials-welding@googlegroups.com
Date: Friday, 8 February, 2013, 1:33 PM

309 is best one

On 2/7/13, Ramin Kondori <raminkondori@gmail.com> wrote:
> Dear Ezat:
>
> As a general recommendation for welding 13%Cr alloy you can use 309 or
> 310 filler metal (I recommend 310 over 309)
> Use preheat of 250-300 degrees and try to maintain it during welding.
> You may need PWHT (holding temperature is higher than 650 degrees)
> based on the thickness of the pipe and your process fluid.
>
> Regards
> Ramin  Kondori
> QC/Welding Engineer
> IWE AT 0070
>
> On 2/7/13, Ezat Adel <ezatadel2008@gmail.com> wrote:
>> Dear Experts,
>>
>> i have to weld  (4 1/16'' 5K) Flange to ( 4'' Api 5L , X 60 ) Pipe, the
>> flange material is 13% cr-110 and the mechanical properties as following:
>>
>> Tensile Strength is 120,000 psi ,Yield Strength is 110,000min. & 130,000
>> max. , Hardness 32 HRC
>>
>>  and the chemical composition as following :
>>   Grade C Si
>> max. Mn P
>> max. S
>> max. Cr Ni Mo Cu
>> max.       13CR -110 max. 0.04 0.50 max. 0.60 0.020 0.010 12.0~14.0
>> 3.50~4.50 0.80~1.50 -
>>
>>  plz send me the proposed welding process and proposed filler metal and
>> thanx for your attention
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...