What contractor says is the best method to achieve result, otherwise
difference in expansion of 2 different materials will play major role
Pandithan
Welding Consultant
On 2/8/13, bijoy joseph <bijoy.joseph1@gmail.com> wrote:
> Dear Dtta,
> You can make grove and plug type joint on the both plates before rolling
> and after rolling remove the eah plug and do the seal welding OR If SS
> plug is aviliale, then can do the seal welding over it.
> Bijoy joseph
>
> On Thu, Feb 7, 2013 at 11:24 PM, c sridhar <sridhar305@yahoo.com> wrote:
>
>> Mr. Dutta,
>>
>> You have mentioned that, 'I would have thought that the flat sheets
>> should
>> be
>> plugwelded to geta single sheet of 36 mm thickness (30 mm SA 516 Grade 70
>> with 6 mmSuperduplex SS lining) and then the entire 36 mm sheet could be
>>
>> rolled. However our contractor informs that there could be problems in
>> the strength of the plug weld and the joints could fail on Rolling.'
>>
>> As you have rightly pointed out, the SS with higher thick CS could be
>> plugged together
>> and then rolled. No problems will arise as long as the weld is sound and
>> with proper fusion..
>>
>> It is a common practice and radiography / Ultrasonic test could be taken
>> at random (or) fully to
>> check the quality of the weld if required.
>>
>> Since you are going to use a SS consumable, the ductility will not be a
>> problem and the rolling
>> will be successful and you can go ahead positively.
>>
>> C Sridhar.
>>
>>
>>
>>
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>>
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>
>> The views expressed/exchnaged in this group are members personel views
>> and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>> ---
>> You received this message because you are subscribed to the Google Groups
>> "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an
>> email to materials-welding+unsubscribe@googlegroups.com.
>> For more options, visit https://groups.google.com/groups/opt_out.
>>
>>
>>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Subscribe to:
Post Comments (Atom)
[MW:34919] Welder qualification certificate
Dear All anyone can share a format for welder certificate and card format Thanks & Best Regards Saleem manhappulath Mob:+9665...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment