Dear Ramachandran 

Check for  hardness at site and prove, identify  raw material heat No and corelate with mtc.   

On Mon, Feb 4, 2013 at 12:50 PM, ratheesh ramachandran <pkrratheesh@gmail.com> wrote:
Dear Experts,


                 I have encountered some problem in my project site.Some NACE material,pipe spools arrived in the site without proper pipe spool identification.Now client is asking to prove that the material is NACE .Some people suggested to cut sample coupon from these pipe spools and sen to laboratory for mechanical tests and whatever tests which are required to prove the NACE conformance.But because of the remote location of the project site,it will be difficult for us to do that within a time limit.So can anyone suggest some method to identify the NACE material,any test which can be carried out in the site itself.

regards
ratheesh.r
ksa

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
Thanks with Regards


Sivayya
S2, Brahma Towers
P.No.65, Palace layout.
 Pedawaltair
VISAKHAPATNAM- 530017 (AP)
Mobile : 9346868777

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...