Friday, February 15, 2013

[MW:16772] RE: 16769] P1 MATERIAL TO 2205 MATERIAL

You may select Avesta 2205 for such dissimilar joining.

 

.You are welcome to visit our web-site thru the link provided below my signature. This will lead you to Avesta site as well which provides  technical inputs & solutions to the challenges in welding of SS , modern DSS & Super duplex SS base materials.

 

With Kind Regards

 

Amitabha Bhattacharya

Head-Application Technology

 

Bohler Welding Group India Pvt. Ltd.

A-140, Road No 23, Wagle Industrial Estate

Metropolitan, Ground Floor

Thane  400 604, India

Ph: +91 22 2582 8855/4228 4400

Mobile ;+91 9833998246

 

Email: amitabha.bhattacharya@bwgindia.com

Web: www.bohlerweldinggroupindia.com

A Böhler Welding Group Company

 

This email message and any attachments are for the sole use of the intended recipient(s) and contain confidential and/or privileged information. Any unauthorized review, use, disclosure or distribution is prohibited. If you are not the intended recipient, please contact the sender by reply email and destroy all copies of the original message and any attachments

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bala Nechur
Sent: Friday, February 15, 2013 9:26 AM
To: materials-welding@googlegroups.com
Subject: [MW:16769] P1 MATERIAL TO 2205 MATERIAL

 

HELLO EXPERTS,

 

i HAVE SOME WELDING 2205 DUPLEX MATERIAL TO P1 GROUP,  FILLET WELD.  PLEASE SUGGEST RECOMMENDED ELECTRODE.

 

BALA

780 204 0239

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...