Dear ,

Attached procedure might help you.

Regards,
Vineet

On Saturday, March 24, 2012 5:36:40 PM UTC+5:30, sandeep monody wrote:
Dear experts,
 
In my site we conducted a demonstration of PWHT on SA335 P91 material (OD-450mm X 70mm Thk) as our clients requirement and details as given below.
 
Heating/cooilng rate;-60 deg C,Holding temparature:-760deg C and holding time:-180minutes,Heating band width:-210mm and insulation band width 630mm,Heating method :-Induction heating
 
During pwht we observed a temparature difference on outside and inside of pipe more than 80 deg C.
 
Now problem is that client is not accepting this method and asking for uniform temparature in outside and inside of pipe.
 
How can i control temparature at both sides?
Is it possible a uniform temp on both side with induction heating?
 
Please give ur valueble advice in this matter.
 
 
Sandeep.
QC Engr

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...