Wednesday, February 13, 2013

[MW:16755] Pull out Test Required in Tube to Tubesheet Welding

Respected Experts,

I want to know why we done pullout test in Tube to tube sheet welding and not done in U-tube construction.

As per client specification Pullout is required in one of our job but tube construction is U-tube.

How strength can be established if pullout is required. Job Code applicable is ASME Section III NB class1 components & ASME Section III NC.


Thanks 

Regards
Mohit Aggarwal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...