Dear experts,
As far as I know refering QW-420.2 Asme sec9, when we qualify P1toP1 or P1toS1 it will qualify all P1toP1, P1toS1 and S1toS1
But welding S1toS1 will only qualify S1toS1 materials, is that right?
My question is can we make a WPS from p1g1 to p1g2 PQR to weld for exmpl. API 5L X60 material?
I found different sources that claims x60 as S1 mat or P1 material.
Regards,
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Subscribe to:
Post Comments (Atom)
[MW:34919] Welder qualification certificate
Dear All anyone can share a format for welder certificate and card format Thanks & Best Regards Saleem manhappulath Mob:+9665...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment