Wednesday, November 21, 2012

[MW:15984] Class-II used instead of Class I film

Dear all,

Our RT subcontractor used by mistakes Class-II (kodak)film instead of class-I (Kodak)

Pipe Materials : 8" API 5L GrB  thk : 8.18mm. No of Joints : 35 Joints.

As per Spec : Class-I required for thickness less than 12.7mm.

Client rejects all RT films.

Any possible solution?

regards,
mohd.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...