Re: [MW:16008] welds proximity

Dear Pinaki,

You can find in ASME VIII Div. I, UW-9 (d).
 
(d) Except when the longitudinal joints are radiographed 4 in. (100 mm) each side of each circumferential welded
intersection, vessels made up of two or more courses shall have the centers of the welded longitudinal joints of adjacent
courses staggered or separated by a distance of at least five times the thickness of the thicker plate.

I hope the above is clear.

Regards
Vino-Doha



On Tue, Nov 20, 2012 at 1:31 PM, Pinaki Boxi <boxi.pinaki@gmail.com> wrote:


Dear All,

Can you please confirm if there are any mandatory limitations on weld to weld distance (nozzle to CS/ LS, CS to CS, LS to LS, welds of attachments to other welds etc.)

Details:

Governing code: ASME Sec VIII Dev 1&2 and ASME  B31.3 & 31.1
PWHT – Application on requirement basis.
NDT: 100% &10%  RT & MPI on attachment/ fillet welds.

 

Does a weld meeting all above criteria (2 to 4) have an issue, metallurgically, when welds are too close or don't have even spacing e.g. weld long seam to long seam, (piping) reinforcement pad to  support  etc.


Thanks & regards

Pinaki Boxi.

Paradeep, PDRP Project.

Mob :- 9178466059.


 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...