Using class - II film instaed of class - I film need not be a reason for rejection, provided, if you have achieved the required density and sensitivity. Convince your client and do not repeat it in future.
ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,
Nandesh Kumar A Abu Dhabi, UAE
P.S. : Please don't print this e-mail unless you really need to.
--- On Wed, 21/11/12, mohd <mohd52100@gmail.com> wrote:
From: mohd <mohd52100@gmail.com> Subject: [MW:15984] Class-II used instead of Class I film To: materials-welding@googlegroups.com Date: Wednesday, 21 November, 2012, 9:01 AM
Dear all,
Our RT subcontractor used by mistakes Class-II (kodak)film instead of class-I (Kodak)
Pipe Materials : 8" API 5L GrB thk : 8.18mm. No of Joints : 35 Joints.
As per Spec : Class-I required for thickness less than 12.7mm.
Client rejects all RT films.
Any possible solution?
regards, mohd. -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/ http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments