Dear Sir,
It seems the weld defect is due to i) Welder skill  if it is ok ii) Flux coating of the Electrodes Why not change the brand and try As such these typeE8018B2L  of elctrodes   are being used by many fabricators w/o problems
Please check Current, Voltage and bead placement and also Joint configuration
 
Regards
 
Hegde


--- On Fri, 30/11/12, sudalai kannan <sudalaims@gmail.com> wrote:

From: sudalai kannan <sudalaims@gmail.com>
Subject: Re: [MW:16091] Consumable for SA 387 GR-12.CL2 materials
To: materials-welding@googlegroups.com
Date: Friday, 30 November, 2012, 3:31 PM

Dear sir,

The base material is SA 387 GR12.CL2 it's conformed, we tried with E8018-B2 (ESAB), but the Radiographic reports shown on everywhere is Incomplete fusion, We follow proper Preheat, Interpass & we used the good welder for the joint.

Then only client informed us to use E7018-B2L electrode.

Please give me feed back the above issue.

Thanks to you.

Regards,
M.Sudalai.

On 30 November 2012 08:56, HAREESH K V <hareesh13h@gmail.com> wrote:
Dear Sir,

You can use E7018-B2L of E8018-B2L. Not got a good result? What happened, please explain.


Regards,

Hareesh K V
+8306703707
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...