Dear sir,

The base material is SA 387 GR12.CL2 it's conformed, we tried with E8018-B2 (ESAB), but the Radiographic reports shown on everywhere is Incomplete fusion, We follow proper Preheat, Interpass & we used the good welder for the joint.

Then only client informed us to use E7018-B2L electrode.

Please give me feed back the above issue.

Thanks to you.

Regards,
M.Sudalai.

On 30 November 2012 08:56, HAREESH K V <hareesh13h@gmail.com> wrote:
Dear Sir,

You can use E7018-B2L of E8018-B2L. Not got a good result? What happened, please explain.


Regards,

Hareesh K V
+8306703707

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...