Re: [MW:15999] WQT without WPS

All welds shall be rejected. RT/UT & hydrostatic test are not substitute for such non-conformities.  Any construction code for any type of welds, welding procedure is mandatory.
NDE does not confirm or guarantee the integrity of weld joints. Hydrostatic test does confirm the mechanical properties of Welds as hydro test pressure will be lesser than yield & tensile strength.
Regards

On Wed, Nov 21, 2012 at 11:18 PM, Sudhir Kumar <sudhir18092@gmail.com> wrote:


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...