Sunday, November 25, 2012

RE: [MW:16031] Maximum Operating Temp. for UT

UT @ 1200° C????

UT of what material you are talking about? Hope it is not steel, as you are nearing the melting temperature of steel, which is around 1400° C.

ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,

Nandesh Kumar A

Abu Dhabi, UAE

P.S. : Please don't print this e-mail unless you really need to.


--- On Sun, 25/11/12, Vivek <vivek12787@gmail.com> wrote:

From: Vivek <vivek12787@gmail.com>
Subject: RE: [MW:16027] Maximum Operating Temp. for UT
To: materials-welding@googlegroups.com
Date: Sunday, 25 November, 2012, 9:57 AM

Hey Vino,

Thanks for reply.
But I had also heard that it can also be done at 1200 deg.cel. by using specially designed probe.
I will be very thankful if any one can provide me ASME code reference for d same.

Regards
Vivek V.Mane

-----Original Message-----
From: Vino Varghese
Sent:  24.11.2012, 9:27  PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:16026] Maximum Operating Temp. for UT


Dear Vicky,

It is 52 Degree Centigrade..

Regards
Vino-Doha

On Sat, Nov 24, 2012 at 6:40 AM, Vicky Patil <patilvicky4@gmail.com> wrote:

> Dear Experts,
>
> What is the maximum allowable temperature to carry out UT?
>
> Regards,
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
>
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...