Thursday, November 29, 2012

Re: [MW:16079] What are the criteria to select Stub in or Stub on for Branch connection in Piping?

the branch connection for the header with re-pad should be stub-out. The header that does not have re-pad should be stub-in.

Regards
samir

On Thu, Nov 29, 2012 at 1:47 PM, PK M <pkmqaqc@gmail.com> wrote:
Dear Experts,

What are the criteria to select Stub in or Stub on for Branch connection in Piping?

(Or)

How to choose Stub in or Stub on for Branch connection in Piping?


Thanks,

Pkm..

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
Samir Mehta
Engineer - Welding & Projects
JPIOS
Abu Dhabi - UAE
+971 55 94 25 327

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...