[MW:16032] RE: 16022] PROCEDURE QUALIFICATION - B690 seamless AL6XN pipe (SPEC # SB 366 UNS # N08367)
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist
Gas Tungsten Arc Welding — Shielding and backing gas should be completely inert or contain 3-5% N2 for enhanced corrosion resistance. Argon or argon helium mixes are often used .
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bala Nechur
Sent: Friday, November 23, 2012 11:14 AM
To: materials-welding@googlegroups.com
Subject: [MW:16022] PROCEDURE QUALIFICATION - B690 seamless AL6XN pipe (SPEC # SB 366 UNS # N08367)
Hello Expert,
I like to establish Welding Procedure for the material “ B690 seamless AL6XN pipe (SPEC # SB 366 UNS # N08367) using ERNiCrMo-10 & ENiCrMo-10. I tired with Argon 99.9% shielding gas for root and observed that penetration was not satisfactory, The filler wire is recommended by the client.
Will you please recommend your suggestions and alternate method to get good penetration .
Bala Nechur,
Corporate QA/QC Manager
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments