dear sir,
generally, e 70s-2 we are generally used for gtaw rod
,while er 70s-6 we are using in gmaw
thanks & regards
dinesh
generally, e 70s-2 we are generally used for gtaw rod
,while er 70s-6 we are using in gmaw
thanks & regards
dinesh
On Mon, Nov 26, 2012 at 12:19 PM, Vinu Raveendran <vinuravi007@gmail.com> wrote:
--Dear Members,I would like to know difference between ER70S2 &ER70S6?What does "2" and "6" mean in them and which welding process we use them?Thankyou!
--
VINU RAVEENDRAN
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments