There is insufficient information given to determine whether the substitution would be permissible or not.  The proposed substitution may be permitted provided the following questions can be answered satisfactorily:

·         Is the original flux wire combination classified as per Section II Part C? 

·         Is the original flux;  i.e. same brand and type, to be used with only a change in wire? 

·         Is the original flux  classified with the EL8 wire as per Section II Part C?

·         Is the strength designator of the classifications the same for both flux-wire classifications?

If the answer to all the forgoing is an unqualified YES  then the substitution may be made per QW-404.9 and QW-404.5.

 

I would recommend that care be taken be taken in making such a substitution, but it is possible per Section IX.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of pgoswami
Sent: Monday, November 26, 2012 9:51 PM
To: 'kiran kumar'
Cc: materials-welding@googlegroups.com
Subject: [MW:16046] RE: welding with EL8

 

Hi Kiran,

 

For SAW the wire flux classification is important than filler metal alone. Sec-IX,QW-404.9 addresses this issue.

 

A change from EH14 (1.8% Mn) to EL8( less than 1% Mn) would cause significant reduction in weld metal mechanical properties.

 

Hence this change may not be allowed unless a new PQR is qualified.

 

Thanks.

 

 

Pradip Goswami,P.Eng.IWE

Welding & Metallurgical Specialist

Ontario, Canada.

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 

 


From: kiran kumar [mailto:chvvn.kirankumar@gmail.com]
Sent: Monday, November 26, 2012 3:54 AM
To: pgoswami@sympatico.ca; pgoswami@quickclic.net
Cc: materials-welding@googlegroups.com
Subject: welding with EL8

Dear Sir

 

Can we weld with Filler wire  EL8 with supporting PQR  EH 14 Filler wire (having same F no:6)

 Material IS 2062

 Construction code -BPVC Section IX

 Process-SAW Process.

 

Thanking you

 

CH.V.V.N.KIRANKUMAR

 

+91 7898905072

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...