Hi,
01. For UNS N08800 use AWS ENiCrFe-2
02. For S31625 use E318-15
Also please find herewith the attached files might be useful to you.
Thanks & Regards,
(Karthik)
Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8, Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Fax : +66 38 897 034
Hand Phone: 0066 892512282
From: James cyrilandrew <jcyrilandrew@gmail.com>
To: Material welding groups <materials-welding@googlegroups.com>
Sent: Wednesday, November 28, 2012 1:55 AM
Subject: [MW:16057] Regarding Welding of some materials
To: Material welding groups <materials-welding@googlegroups.com>
Sent: Wednesday, November 28, 2012 1:55 AM
Subject: [MW:16057] Regarding Welding of some materials
Dear All,
-- After a long time i am here with some clarifications....... I hope i will get a detailed reply....... the doubt is,
1. Material Number- 1.4876 and UNS N08800.
2. Material Number- 1.4571 (316Ti)..... and its UNS S31625
for the above materials what is the electrode specification, class and whether heat treatment is there or not and how abt shielding gas....
pleaseclarify... awaiting for reply..... thank you.
--
Regards,
Cyril
Doha-Qatar
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments