Re: [MW:16047] DIFFERENCE BETWEEN ER70S-2 &ER70S-6

Both are useing for gtaw. 70s6 contains more si.which is  good for welding in highly contaminated area

On Nov 26, 2012 8:54 AM, "Dinesh Somwanshi" <som.din@gmail.com> wrote:
dear sir,

generally, e 70s-2 we are generally used for gtaw rod
,while er 70s-6 we are using in gmaw

thanks & regards

dinesh


On Mon, Nov 26, 2012 at 12:19 PM, Vinu Raveendran <vinuravi007@gmail.com> wrote:
Dear Members,

I would like to know difference between ER70S2 &ER70S6?
What does "2" and "6" mean in them and which welding process we use them?

Thankyou! 

--
VINU RAVEENDRAN

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...