Re: [MW:16013] Level II in ultrasonic thickness gauging

thickness measurement by using UT gauge, ASNT Level II is mandatory, ASNT Level II in UT will qualify thickness measurement also.
 
Regards
Sudhir Kumar

On Fri, Nov 23, 2012 at 10:50 AM, HAREESH K V <hareesh13h@gmail.com> wrote:
Dear Sir,

Is there ASNT level II in ultrasonic thickness gauging (UTTG)?

If so where i can do it in india?

Thanks in advance,

----------------------
Hareesh K V
+91-9447625012


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...