Re: [MW:16060] DIFFERENCE BETWEEN ER70S-2 &ER70S-6

ER 70S2-------- Triple Deoxidiser ( Ti, Al, Zr). This is mostly used in GTAW process and not in GMAW process due to loss of Titanium in arc column.

ER70S6------- Highly Deoxidiser With High Mn & Si. This is mostly used in GMAW process.

Pandithan
welding consultant

On Mon, Nov 26, 2012 at 1:49 PM, Vinu Raveendran <vinuravi007@gmail.com> wrote:
Dear Members,

I would like to know difference between ER70S2 &ER70S6?
What does "2" and "6" mean in them and which welding process we use them?

Thankyou! 

--
VINU RAVEENDRAN

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...