Dear Everybody,
Can you give me light on which film is Type 1 & which is type 2. Agfa
d4 comes under which catagory.
Regards
Pradip
On 11/21/12, mohd <mohd52100@gmail.com> wrote:
> Dear all,
>
> Our RT subcontractor used by mistakes Class-II (kodak)film instead of
> class-I (Kodak)
>
> Pipe Materials : 8" API 5L GrB thk : 8.18mm. No of Joints : 35 Joints.
>
> As per Spec : Class-I required for thickness less than 12.7mm.
>
> Client rejects all RT films.
>
> Any possible solution?
>
> regards,
> mohd.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Can you give me light on which film is Type 1 & which is type 2. Agfa
d4 comes under which catagory.
Regards
Pradip
On 11/21/12, mohd <mohd52100@gmail.com> wrote:
> Dear all,
>
> Our RT subcontractor used by mistakes Class-II (kodak)film instead of
> class-I (Kodak)
>
> Pipe Materials : 8" API 5L GrB thk : 8.18mm. No of Joints : 35 Joints.
>
> As per Spec : Class-I required for thickness less than 12.7mm.
>
> Client rejects all RT films.
>
> Any possible solution?
>
> regards,
> mohd.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments