Re: [MW:15817] Dissimilar welding CS to DUPLEX SS

Hi,

I would use E309 for this thickness, no preheating, maximum interpass temperature is 150 deg C


Regards,
Manpreet Singh



On Tue, 30 Oct 2012 14:17:45 +0530 wrote
>Dear Experts,

In our isometric drawing shows dissimilar welding carbon steel to

duplex stainless steel ( 31254 grade ) thk is 9.52 mm. Can anybody

give me guideline to make this WPS.

Regards

Pradip



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm



The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.







Catch India as it happens with the Rediff News App. To download it for FREE, click here

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...