RE: [MW:15807] Can we measure the Ug

Dear all,

 

T-274.1 Geometric Unsharpness Determination.

Geometric unsharpness of the radiograph shall be determined in accordance with:

 

Ug = Fd/D

 

where,

 

Ug = geometric unsharpness

 

F = source size: the maximum projected dimension of the radiating source (or effective focal spot) in the plane perpendicular to the distance D from the weld or object being

      radiographed

D = distance from source of radiation to weld or object being radiographed d p distance from source side of weld or object being radiographed to the film D and d shall be determined

      at the approximate center of the area of interest.



Please refer Sec -V ASME for more details.


 


Thank & Best Regards,

 

M Veera SAMY- Bureau Veritas.

Coimbatore

 

 


 

Date: Tue, 30 Oct 2012 09:39:55 +0530
Subject: [MW:15801] Can we measure the Ug
From: nagarajanqc187@gmail.com
To: materials-welding@googlegroups.com

Dear Experts,
                      
                        Can we measure the Ug in RT interpretitation ? If Yes , How to measure tell me
 
 
with regaeds
 
nagu

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...